Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 20.0 microns | 0.787 mil | |
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Thickness | 20.0 microns | 0.787 mil | |
NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Thickness | 20.0 microns | 0.787 mil | |
NOVA Chemicals Sclair® FG220-A Octene LLDPE Film Resin Features: Exceptional toughnessLow gel level Applications: Cast stretch wrapNettingCo-extrusion and laminationInformation provided by Nova Chemicals |
|||
Thickness | 20.0 microns | 0.787 mil | |
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou.. |
|||
Thickness | 20.0 microns | 0.787 mil | As tested for properties on this data sheet |
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Thickness | 20.0 microns | 0.787 mil | |
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin Features: Exceptional puncture resistanceVery good tear propertiesLow gel levelExcellent optical properties Excellent elongation characteristics Easy to process, no drying required Applications: Cas.. |
|||
Thickness | 20.0 microns | 0.787 mil | extruded at 750ft/min take off speed and melt temperature of 274-302°C |
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin
(discontinued **) Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng.. |
|||
Thickness | 20.0 microns | 0.787 mil | |
NOVA Chemicals Novapol® PF-0318-E Butene LLDPE Film Resin PF-0318-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 20 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 20 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 20 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 20 µm) HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead ML11 General Grade BOPP Matt Film (thickness: 20 µm) ML11 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. One side has corona treatment. It is specially designed for board laminati.. |
|||
Thickness | 20.0 microns | 0.787 mil | ± 3.0%; ASTM-252-78 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 20 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |
|||
Thickness | 20.0 microns | 0.787 mil | As tested |
Metabolix M-veraâ„¢ B5008 Film Grade Compostable Bioplastic B5008 is a compostable film product with 30% biobased carbon content that is ideal for compost bags and can liners used for organic waste diversion and for shopping and retail bags.Features:Meets re.. |
|||
Thickness | 20.0 - 100 microns | 0.787 - 3.94 mil | |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Thickness | 20.0 microns | 0.787 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS1500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | |
Gwent Electronic Materials C2030325D14 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Thickness | 20.0 - 100 microns | 0.787 - 3.94 mil | possible range, depending on extrusion conditions |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Thickness | 20.0 - 100 microns | 0.787 - 3.94 mil | possible range, depending on extrusion conditions |
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch.. |
|||
Thickness | 20.0 - 150 microns | 0.787 - 5.91 mil | possible range, depending on extrusion conditions |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Thickness | 20.0 microns | 0.787 mil | |
Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film Lumicene® mPE M 4040 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 4040 can be processed at high output rates with low extrusion pressure, low neck-in, ex.. |
|||
Thickness | 20.0 microns | 0.787 mil | |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Thickness | 20.0 microns | 0.787 mil | |
Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Thickness | 20.0 microns | 0.787 mil | 4:1 blow-up ratio |
Bapolene® 350F Polyethylene, Film Grade Applications: Blown film extrusion of T-shirt sacks, merchandise bags.Film properties below are based on a thickness of .8 mil and blow-up ratio of 4:1.Bapolene® and Bapolan® are registered tradem.. |
|||
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | |
Gwent Electronic Materials C2040226D2 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | |
Gwent Electronic Materials C2040226D4 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Thickness | 20.0 microns | 0.787 mil | Double layer on 175µm ITO coated polyester |
Gwent Electronic Materials D2090130P5 Pink Dielectric Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |