Processing Properties Metric English Comments
Processing Temperature >= 20.0 °C
>= 68.0 °F
3M Scotch-Weld™ 3549 B/A Brown Two-Part Urethane Adhesive 3549 B/A Brown  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include long worklife adhesive, 2-4 hours handling stren..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.30% glass-fiber, general purposeInformation provid..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2001 PBT  (Unverified Data**)
Celanex 2001 is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications. Celanex 2001 exhibits the high melt st..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2302 GV1/30 PBT, 30% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: PBT30% glass fiber reinforced, high glossInformation provided by Celanese
Processing Temperature 20.0 °C
68.0 °F
Average value: 20.0 °C Grade Count:30
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Processing Temperature 20.0 - 230 °C
68.0 - 446 °F
Average value: 160 °C Grade Count:25
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 2521 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMStiff-flowing grade for injection molding and extrusionInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 2521 XAP² ™ POM  (Unverified Data**)
POM copolymerlow EmissionInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 AW XAP² ™ LS POM, Tribological  (Unverified Data**)
POM copolymerLow noise, low wear and low emissionsInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 K POM, Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with special chalk modifiedInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological  (Unverified Data**)
POM copolymerTribological, Low EmissionInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® M25AE POM  (Unverified Data**)
Hostaform® M25AE is a special grade of acetal copolymer targeted for extrusion shapes (rod, bar, plate, etc) free of center porosity in large diameters and thicknesses.Extrusion grade targeted for ..
Processing Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Celanese VECTRA S625 LCP, 25% Specialty  (Unverified Data**)
Low friction and wear resistance.Low friction and wear resistance.Information provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 309 PPS  (Unverified Data**)
0309 exhibits a good balance of flow and melt strength for extrusion processes. The material demonstrates excellent heat and chemical resistance. The intended use of this product is for extruding mo..
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced  (Unverified Data**)
Fortron 1140L4 is a 40% glass-reinforced grade that is the strongest and toughest product available. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently ..
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 1342L4 PPS, 40% Specialty  (Unverified Data**)
Fortron 1342L4 is a low wear grade, ideally suited for bearings, gears and other sliding friction/wear applications. This product is glass fiber reinforced and contains PTFE.40% Glass reinforced wit..
Processing Temperature 20.0 °C
68.0 °F
typically used at ambient temperature
Elmer's Products Aron Alpha® 203 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair o..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3318 PBT, 30% Glass Reinforced
Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Processing Temperature 20.0 - 55.0 °C
68.0 - 131 °F
cavity
Celanese RITEFLEX 425 TPC, Unfilled
Riteflex 425 is a nominal 25 Shore D thermoplastic polyester elastomer with low modulus and outstanding low temperature impact, and tear resistance.Information provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 GV1/10 POM, 10% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 10 % glass fibersInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 GV3/10 POM, 10% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 10 % glass spheresInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 GV3/20 POM, 20% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 20 % glass spheresInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 SW POM, Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, special modified with anti-friction additives for prevention of squeaking noiseInformation provided by Celanese
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® MT12U01 POM, Medical Technology  (Unverified Data**)
Hostaform® MT12U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT12U01 is a moderately high flow grade for fa..
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON MT9140L4 PPS, 40% Medical Technology  (Unverified Data**)
Fortron MT 9140L4 is a 40% glass fiber reinforced injection molding grade that exhibits excellent heat and chemical resistance, inherent flame retardancy, and high hardness and rigidity at elevated..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1400FC PBT  (Unverified Data**)
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3309HRT PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.30% glass reinforced, unlubricated, hy..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Vandar® 2100UV PBT, Impact Modified  (Unverified Data**)
Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional sta..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Impet® 340R PET, 45% Glass Reinforced  (Unverified Data**)
Impet 340R is a 45% glass-reinforced injection moldable polyester made with post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.4..
Processing Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 4184L4 PPS, 53% Mineral / Glass Reinforced  (Unverified Data**)
Fortron 4184L4 is the strongest and toughest glass/mineral reinforced product available. It offers excellent heat resistance at high loads and good chemical resistance. The electrical properties are..