Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ISO 527-3
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene
Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ISO 527-3
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
Reliance Industries LLDPE film - Organic acid based film
Information provided by Reliance Industries
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PPE 1461  (discontinued **)
PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D882
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D 882
NOVA Chemicals Novapol® PF-0118-DP Butene Copolymer LLDPE Film Resin
PF-0118-DP complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatu..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ISO 527-3
Borealis FG5190 Linear Low Density Polyethylene
FG5190 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes Antioxidant. The grade is developed for medium and heavy duty bags, bags and bin liners, dual stretch films, and film..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
50 µm (2 mil) film; ASTM D882
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown
12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ISO 527-3
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308FK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processabilityIncreased stiffnessGood toughnessUse alone or in blends with LDPE o..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM-D882
Braskem TN2005 EVA General Film Copolymer
TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D-882
Bapolene® 152A Polyethylene Film Grade
Bapolene 152A is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products...
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D-882
Bapolene® 152B Polyethylene Film Grade
Bapolene 152B is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products...
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D-882
Bapolene® 152F Polyethylene Film Grade
Bapolene 152F is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products...
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D882
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio..
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D882
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin  (discontinued **)
Applications: Lamination Film, coextruded sealant layer, high toughness filmInformation provided by Nova Chemicals
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D882
Chevron Phillips 7105DKT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Antiblock, Processing Aid Version of 7105T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..