Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D2030210D1 Polymer Dielectric This material is a black colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D50706D2 Polymer Dielectric This material is a cream colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D50706P3 Polymer Dielectric This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode... |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials G2020520D1 Gold Metallo-Organic Ink This is a screen printing ink designed to act as a working electrode when fired onto alumina substrates. This unique MO formulation gives a fired thickness in the order of 0.2 to 0.3 microns. This.. |
|||
Processing Temperature | 65.0 - 80.0 °C @Time 900 sec |
149 - 176 °F @Time 0.250 hour |
|
Henkel Turco 5948-R Deoxidizer Turco 5948-R is an alkaline, water-based, blue, concentrated compound formulated to effectively clean painted and unpainted aircraft exterior and interior surfaces when diluted with water. Ideally s.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Hopper |
Eurostar Staramide PX08000 PA6, Impact Modified, Injection Molded Staramide PX08000 is an Impact Modified Polyamide 6 Injection Molding Resin (also known as Star X 2006)Information provided by Eurostar. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Hopper |
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Processing Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |
|||
Processing Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Henkel Turco 6776-LO Paint Remover Turco 6776-LO environmentally advantaged paint remover is low-odor, thixotropic, developed for effective stripping of such resistant finishes as epoxies, epoxy primers, polyurethanes and similar cat.. |