Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance .. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East) GELOY HRA170 is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour .. |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525B |
SABIC PP 623B Polypropylene Random Co-polymer for Cast Film Product Description: PP 623B is a PP Random Copolymer grade specially designed for Cast PP (CPP) film extrusion. It contains slip agent and anti-block additives. PP 623B offers good heat weldabil.. |
|||
Vicat Softening Point | 132 °C | 270 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND PCA PD 935 G4 PC+ABS, 20% Glass Fiber
(discontinued **) Symbol according to ISO 1043/1/2: PC+ABS (GF) Injection moulding grade, reinforced with 20% glass fibres, high stiffness, very good dimensional stability. Main application fields: structural non a.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525 |
Ineos A60-70-162 HDPE Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525 |
Ineos K50-10-136 HDPE Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished produc.. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East) VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific) LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |
|||
Vicat Softening Point | 132 °C | 270 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East) Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating .. |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Vicat Softening Point | 132 °C | 270 °F | A50; ISO 306 |
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
Vicat Softening Point | 132 °C | 270 °F | A (10N); ISO 306 |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Unipetrol PP MONSTEN® MT 812 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 132 °C @Load 5.00 kg |
270 °F @Load 11.0 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 132 °C @Load 5.00 kg |
270 °F @Load 11.0 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND PSA 7800 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 132 °C | 270 °F | 50°C/hr; 50N |
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Vicat Softening Point | 132 °C | 270 °F | B/50; ISO 306 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525 |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 132 °C | 270 °F | ASTM D1525 |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 132 °C @Load 1.02 kg |
270 °F @Load 2.25 lb |
ASTM D1525 |
Carmel Olefins CAPILENE® QM 45 F Propylene Random Copolymer Description: CAPILENE® QM 45 F is a slip and anti-block formulated random copolymer. It is characterized by high gloss and easy processing.Applications: CAPILENE® QM 45 F is suitable for cast u.. |
|||
Vicat Softening Point | 132 °C | 270 °F | ISO 306 |
Unipetrol PP MONSTEN® FC 908 Polypropylene Random Copolymer Applications include injection molding and packaging films. Slip and antiblocking agent stabilization. Random copolymer.Information provided by Unipetrol RPA |