Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Glass + PTFE Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced, PTFE Lubricated
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.080 %
0.080 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Ultimate 117 MPa
17000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Compressive Yield Strength 110 MPa
16000 psi
ASTM D695
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.59 mm
V-1

@Thickness 0.0625 in