Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled , Polycarbonate, Impact Modified
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Melt Flow 30 g/10 min

@Load 10.0 kg,
Temperature 250 °C
30 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 78.5 MPa
11400 psi
5 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
2.8 mm/min; ASTM D790
Flexural Modulus 3.73 GPa
540 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.785 J/cm

@Thickness 3.17 mm
1.47 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C

@Thickness 6.40 mm
275 °F

@Thickness 0.252 in
ASTM D648