Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | |
LATI Later 4 G/30-V0HF1 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, Conditioned Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp WBG16 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WBG16 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Graphite.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 L BN047 LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: BeigeInformation.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI LNP* THERMOCOMP* ECF62 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI (Asia Pacific) LNP* Thermocomp* ECF62 is a compound based on Polyetherimide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PA6/6,6 GF50 HS L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 (Asia Pacific) LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific) LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East) LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RZ0069 PA 66 (Asia Pacific) LNP* Thermocomp* RZ0069 is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant, Milled Glass. Added features of this material include: Flame Retardant. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Plenco 00732 Melamine-Phenolic, Granular, Injection Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Plenco 3356 Phenolic, Granular, Transfer Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
DSM Arnite® TV4 270 PBT-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.57 g/cc @Temperature 23.0 °C |
0.0567 lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
Ensinger TECASINT 1031 Polyimide, 40% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.57 - 1.61 g/cc | 0.0567 - 0.0582 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 88/3 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 528L-50G Nylon 66, 50% Glass Reinforced A general purpose 50% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Density | 1.57 g/cc @Temperature 23.0 °C |
0.0567 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |