Polymer Property : Compressive Yield Strength = 110 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 110 - 138 MPa
16000 - 20000 psi
Average value: 120 MPa Grade Count:7
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Compressive Yield Strength 110 - 380 MPa
16000 - 55100 psi
Average value: 237 MPa Grade Count:63
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Compressive Yield Strength 110 MPa
16000 psi
10% Deflection; ASTM D-695
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin
Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p..
Compressive Yield Strength 110 MPa
16000 psi
Cytec Thornel® Graphite Cloth Laminate with Mil R-9299 Resin
Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature..
Compressive Yield Strength 110 MPa

@Strain 10.0 %,
Temperature 23.0 °C
16000 psi

@Strain 10.0 %,
Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT™ 2032 Polyimide, Black, 40% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Compressive Yield Strength 110 MPa
16000 psi
ASTM D695
Adell AJ-13 Nylon 66, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 110 MPa
16000 psi
ASTM D695
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 110 MPa
16000 psi
ASTM D695
Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated
30% Glass Reinforced, PTFE Lubricated
Compressive Yield Strength 110 MPa
16000 psi
Average value: 110 MPa Grade Count:3
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Compressive Yield Strength 110 - 124 MPa
16000 - 18000 psi
Average value: 114 MPa Grade Count:4
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..