Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Hexene Copolymer, High Antiblock Version of 7109TCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Garment Bags, Carrier Bags, CoextrusionsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.1905 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm. Antiblock 6500 ppm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 0.90 g/10 min
0.90 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.250 GPa
36.3 ksi
ASTM D882
Secant Modulus, TD 0.310 GPa
45.0 ksi
ASTM D882
Coefficient of Friction 0.60
0.60
ASTM D1894
Dart Drop 4.70 g/micron
119 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D2457
Gloss 60 %
60 %
at 45°. ASTM D 2457
100 %
100 %
at 60°. ASTM D 2457
Processing Properties Metric English Comments
Melt Temperature 220 °C
428 °F