Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 5163X0085 0.0085" (0.216 mm) Cured Silicone Rubber with Fiberglass Substrate  (discontinued **)

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 5163X0085 0.0085" (0.216 mm) Cured Silicone Rubber with Fiberglass Substrate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50 inches Overall Width. Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberProduct Description: Acoustical dampeningAppearance: Silver silicone on fiberglass clothThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Side 2
127 microns
5.00 mil
Side 1
191 microns
7.50 mil
7628 Fiberglass, Substrate
191 - 241 microns
7.50 - 9.50 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 25 - 35
25 - 35
Compound Property
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Elongation at Break >= 250 %
>= 250 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test <= 3.0
<= 3.0
[in], Char Length; FTMS 191A; Method 5903
<= 25
<= 25
[sec], Flame and Glow Time; FTMS 191A; Method 5903
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.9 °C
60.0 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Aluminum
Total Product Weight (oz/yd2) 6.7 - 8.1
Uncoated Fabric Break Strength 200 lb/in
Fill Direction, Substrate Property
250 lb/in
Warp Direction, Substrate Property
Users viewing this material also viewed the following: