Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Manufacturer Techmer ES
Trade Name Electrafil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 172 MPa
25000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 221 MPa
32000 psi
ASTM D790
Flexural Modulus 21.7 GPa
3150 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 266 °C
510 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10 - 100 ohm-cm
10 - 100 ohm-cm
ASTM D648
Surface Resistivity per Square 100 - 1000 ohm
100 - 1000 ohm
ASTM D648