Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 10 ohm-cm @Thickness 0.400 mm |
<= 10 ohm-cm @Thickness 0.0157 in |
ISO D-257 |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D257 |
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D257 |
PolyOne Lubri-Tech™ PK-30CF/10T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 10 ohm-cm | 10 ohm-cm | |
Radici Radilon® A RCF3505 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | <= 10 ohm-cm | <= 10 ohm-cm | VDE 0303 |
GEHR Plastics POM-ELS Acetal, Electrically Conductive Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D648 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS |
|||
Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D648 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS |
|||
Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D648 |
Techmer ES Electrafil® M-1322 PA66 / PA6 |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 CF20 TL15 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance:.. |
|||
Volume Resistivity | 10 - 10000 ohm-cm | 10 - 10000 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta.. |
|||
Volume Resistivity | 10 ohm-cm | 10 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PPA CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6 CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Conductive and LubricatedAppearance: BlackInform.. |
|||
Volume Resistivity | 10 ohm-cm | 10 ohm-cm | 25% Carbon Black in HDPE |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Volume Resistivity | <= 10 ohm-cm | <= 10 ohm-cm | IEC 93 |
CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D648 |
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |