Polymer Property : Surface Resistivity per Square = 1000 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced  (discontinu
Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated  (discontinued
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 800 - 1000 ohm
800 - 1000 ohm
prints from standard 140/31 screen
Heraeus Cleviosâ„¢ S HT Antistatic/Conductive Polymer Coating for Screen Printing
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as a paste designed for application by silk screen printing to be used for transparent conductive devices. Cleviosâ„¢ S HT grade ..
Surface Resistivity per Square 100 - 1000 ohm
100 - 1000 ohm
ASTM D648
Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS
Surface Resistivity per Square 100 - 1000 ohm
100 - 1000 ohm
ASTM D648
Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS
Surface Resistivity per Square 100 - 1000 ohm
100 - 1000 ohm
ASTM D648
Techmer ES Electrafil® NY-3/EC BK PA6
Surface Resistivity per Square 100 - 1000 ohm
100 - 1000 ohm
ASTM D648
Techmer ES Plaslube® J-1/CF/15/TF/20 NAT PA66
Surface Resistivity per Square 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Surface Resistivity per Square 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated  (discontinued
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.