Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D 792 |
SABIC Innovative Plastics Cycolac® INP449 SAN SABIC INP449 is a T-SAN (Teflon (PTFE)-Styrene-Ancrylonitrile) resin for use as an FR anti-drip agentThis data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding 40% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin Extem XH2315 Resin |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Specific Gravity | 1.52 - 1.56 g/cc | 1.52 - 1.56 g/cc | ASTM D 792 |
Karina Karintox ENCH./03 Polyolefin Compound Karintox is a thermoplastic polyolefin, flame retardant, non-halogen, and low smoke emission. Recommended for electrical coating for cables until 1KV. For a better usage/processing, a pre-warm/heat .. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface Feature: Injection Molding, PA66+GF46%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base PlateCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | |
MTI ThermoStran® TPU-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | |
Sylvin Technologies 9980-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D297, 15 |
Seals Eastern 7282 Neoprene / Chloroprene UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Beige 6027E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 6027E is a beige color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® is heavy me.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8350 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8350 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
Adell DR-18 40% Glass Reinforced Polycarbonate |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
PolyOne Geon™ CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC) Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excelle.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Bright While LL80250 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL80250 is a bright white masterbatch containing 50% titanium dioxide based in LLDPE. This product has been formulate to provide a brighter, cooler, more fresh appearance ove.. |
|||
Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |