Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |
PolyOne Edgetek® RA-20CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ AT-15CF/5T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **)&l Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |
PolyOne Edgetek® AS-13CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | <= 100 ohm | <= 100 ohm | Dried at 80ºC for 10 minutes then cured at 150ºC for 30 minutes |
Lord Adhesives Metech 2232 Silver Conductor This product is a silver bearing, thermoplastic, acrylic, polymer paint designed primarily as a conductive electrode solder base for tantalum capacitors. Additionally, this material can be used as a.. |
|||
Surface Resistivity per Square | <= 100 ohm | <= 100 ohm | cured; 25 microns thick |
Gwent Electronic Materials C2030325D14 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D648 |
Techmer ES Electrafil® J-4/25/CF/15 BK PA6/12 |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D648 |
Techmer ES Electrafil® J-4/25/CF/15 NAT PA6/12 |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Electrafil® NY-3/EC BK PA6 |
|||
Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |
Techmer ES Plaslube® J-1/CF/15/TF/20 NAT PA66 |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D648 |
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(discontinue Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |
PolyOne Edgetek® PI-20GM-20CF/000 Polyetherimide (PEI), Carbon/Glass Filled
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedCarbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated
  Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® AM-20CF-20GF/000 Polyphthalamide (PPA), Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 ohm | 100 ohm | Typical, Printed through 230 stainless steel mesh with 13 micron emulsion |
Gwent Electronic Materials C2000802P2 Carbon Graphite Ink This product is designed to be used for screen-printing working electrodes. This ink has been optimized to give superior electrochemical performance. It combines good line definition and good electr.. |