Styron TYRILâ„¢ 875 SAN Resin

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer Styron
Trade Name TYRIL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron TYRILâ„¢ 875 SAN Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications. The key property of TYRIL 875 is specifically designed to provide good processability, good chemical resistance, heat resistance, very good strength and optimal aesthetics. Applications: Small appliance: transparent kitchen-robot partsInformation provided by Styron
Physical Properties Metric English Comments
Apparent Bulk Density 0.690 g/cc
0.0249 lb/in³
ISO 60
Melt Flow 6.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527-2/50
Tensile Modulus 3.70 GPa
537 ksi
ISO 527-2
Flexural Strength 97.0 MPa
14100 psi
3 points, 2 mm/min; ISO 178
Charpy Impact Unnotched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 101 °C
214 °F
Annealed; ISO 75-2/A
Vicat Softening Point 111 °C
232 °F
ISO 306/A120
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Users viewing this material also viewed the following: