Solvay ALKAQUAT® DMB-451 80% Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAQUAT®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAQUAT® DMB-451 80% Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: Alkyl Dimethyl Benzyl Ammonium ChlorideCAS: 68424-85-1 Water Solubility: SolubleAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAQUAT© DMB-451 80% is a quaternary biocide and corrosion inhibitor. ALKAQUAT© DMB-451 80% is used in areas such as oil field and industrial applications. In addition to being a corrosion inhibitor, it also has typical surfactant properties that may be a benefit in a given formulation (i.e. wetting, surface tension reduction, particulate dispersion, etc.) Breaker, Corrosion inhibitor, Detergent, Dispersant, Emulsifier, Foam control agent, Gellant, Scale Control, Shale stabilizer, SolventInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
pH 6.0 - 9.0
6.0 - 9.0
10% Solution; RP-0420
Processing Properties Metric English Comments
Moisture Content <= 15 %
<= 15 %
Karl Fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
at 22°C, RP-0064
Colorless to Pale Yellow Liquid
Composition Active
80-83% (EQ. WT. 359.6), RP-0025
Odor Alcohol-like