Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.70 GPa | 537 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
Nylacast Moly Cast Nylon 6, MoS2 Filled Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Nilit FRIANYL A63 SG10 Nylon 6.6 for injection molding, 10% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Nilit FRIANYL A63 KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527-1/-2 |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Manifattura Cattaneo PET Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | |
LATI Latistat 66-06 PA66 Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK) KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing 20% Milled Glass. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC (Asia Pacific) LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing Glass Fiber. Also known as Thermocomp DF-1004 M |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
Styrolution Luran® 358 N SAN Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
Teijin Panlite® G-3410R Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
Teijin Panlite® GN-3410R Improved Mold Release, Glass Fiber Reinforced, Flame Resistant Polycarbonate Resin GF 10% reinforced, flame retardant and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machin.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527-2 |
Styron TYRILâ„¢ 875 SAN Resin Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin HexPly® 954-6 is a 250°F (121°C) curing toughened cyanate resin with 300°F (149°C) Tg. HexPly® 954-6 is formulated for autoclave curing. Recommended cure is three hours at 250°F (121°C). Ser.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ASTM-D790 |
Polyram PlusTek PB351I6 Nylon 6, 30% Glass Fiber and Mineral 30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled PP copolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K224-PG2 PA6-I-GF8 8% Glass Reinforced, Impact Modified |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AS/2 PA66 Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 i.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BS V0 PA6 Product description: Grilon BS V0 is an unreinforced, normal viscosity, self-extinguishing PA6 injection molding grade. Grilon BS V0 has the following important properties: Halogen and phosphorous-f.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | same value from ASTM and ISO test. |
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Dry)
(discontinued **) Capron 5202CQ HS Blend is a heat stabilized, blended polyamide 6,6 injection molding homopolymer developed for fast molding cycles. It is also available in pigmented versions.Capron 5202CQ HS Blend.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |