Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.690 g/cc | 0.0249 lb/in³ | ASTM D1895 |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Apparent Bulk Density | 0.690 g/cc | 0.0249 lb/in³ | ISO 60 |
Styron TYRILâ„¢ 875 SAN Resin Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications.. |
|||
Apparent Bulk Density | 0.690 - 0.720 g/cc | 0.0249 - 0.0260 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Apparent Bulk Density | 0.690 g/cc | 0.0249 lb/in³ | |
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |