Material Notes:
Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable in existing moulds and equipment and can be coloured vividly.Bioplast 2189 is a natural replacement for PVC, PP, HDPE and PET. It is a bio-compostable material made from over 60% sustainable crop material and 20% non oil-based products.Made from corn starch mixed with other proprietary brand products for superior flexibility, Bioplast 2189 polymer is certified EN 13432 and DIN CERTCO biodegradable and compostable. Bioplast 2189 has EU & FDA (USA) Food Contact Approval.Bioplast 2189 was developed for the packaging, consumer and industrial sectors. Applications include formed parts and film usage, i.e. trays, pouches, wrapping, parts, lids, cups and containers. The product is versatile and can be made into sheet for thermoforming, blown into thin sheet for film, or injection moulded into virtually any shape. Bioplast 2189 has the ability to ‘drop into’ most applications with little adjustment or affect on performance.Information provided by Stanelco.
Physical Properties Metric English Comments
Bulk Density 0.880 - 0.940 g/cc
0.0318 - 0.0340 lb/in³
DIN 53466
Density 1.20 - 1.40 g/cc
0.0434 - 0.0506 lb/in³
DIN 53479/A
Melt Density 1.10 - 1.30 g/cc
0.0397 - 0.0470 lb/in³
DIN 53735
Particle Size 2000 - 3000 µm
2000 - 3000 µm
Diameter per caliper rule
Oxygen Transmission Rate 40.0 - 60.0 cc/m²/day
2.58 - 3.86 cc/100 in²/day
400 µm; ASTM F1927-98
Carbon Dioxide Transmission 60.0 - 80.0 cc-mm/m²-24hr-atm
152 - 203 cc-mil/100 in²-24hr-atm
400µm; ASTM D1434
Thickness >= 10.0 microns
>= 0.394 mil
DIN 53353
Melt Flow 15 - 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 - 40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
DIN 53735
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 10 - 30 %
10 - 30 %
DIN 53455
Film Elongation at Break, TD 10 - 30 %
10 - 30 %
DIN 53455
Film Tensile Strength at Break, MD 30.0 - 45.0 MPa
4350 - 6530 psi
50% RH; DIN 53455
Film Tensile Strength at Break, TD 30.0 - 45.0 MPa
4350 - 6530 psi
50% RH; DIN 53455
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
BIOTEC Test
Shelf Life 6.00 Month
6.00 Month
with proper storage