Polymer Property : Apparent Bulk Density = 0.0249 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.690 g/cc
0.0249 lb/in³
ASTM D1895
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Apparent Bulk Density 0.690 g/cc
0.0249 lb/in³
ISO 60
Styron TYRILâ„¢ 875 SAN Resin
Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications..
Apparent Bulk Density 0.690 - 0.720 g/cc
0.0249 - 0.0260 lb/in³
IS 867-1963
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App..
Apparent Bulk Density 0.690 g/cc
0.0249 lb/in³
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..