Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) LF0190 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) LF0190 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LF01090 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: general pupose film and for amination.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ISO 527
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ISO 527
Elongation at Break 100 %
100 %
ISO 527, MD
500 %
500 %
ISO 527, TD
Modulus of Elasticity 0.190 GPa
27.6 ksi
MD; ISO 527
Tensile Impact 200 J/cm
375 ft-lb/in
ASTM D4272
Coefficient of Friction 1.0
1.0
ASTM D1894
Tear Strength 25.0 kN/m
143 pli
TD; ISO 6383-2
70.0 kN/m
399 pli
MD; ISO 6383-2
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003A
Gloss 53 %
53 %
ASTM D2457
Descriptive Properties Value Comments
Clarity, mV 26
Sabtec
Users viewing this material also viewed the following: