Solvay TECHNYL® A 230 PA66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 230 PA66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced and modified polyamide 66, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 230 offers excellent combination between rigidity and impact resistance at ambient temperature. This property save special conditioning before use parts (water absorption). This grade is commonly used for supple parts, such as: fasteners cable ties. This product is available in natural, grey and black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527 Type 1A
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527 type 1 A
Elongation at Break 100 %
100 %
ISO 527 Type 1A
Elongation at Yield 15 %
15 %
ISO 527 type 1 A
Tensile Modulus 1.40 GPa
203 ksi
ISO 527 Type 1A
Flexural Strength 47.0 MPa
6820 psi
ISO 178
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.2
3.2
IEC 60250
Dielectric Strength 16.0 kV/mm
406 kV/in
IEC 60243
Dissipation Factor 0.10
0.10
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %