Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials FSE7540 Heat Cured Fluorosilicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials FSE7540 Heat Cured Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.Fluorosilicones are suitable for applications in presence of fuel, oils, blow by gas, and various solvents. FSE7540 is a peroxide curable, general purpose grade silicone elastomer.All Fluorosilicones are available as customized ready-to-use products.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
Tensile Strength 8.30 MPa
1200 psi
Elongation at Break 380 %
380 %
Tear Strength 13.0 kN/m
74.2 pli
Die B
Compression Set 8.0 %
8.0 %
Descriptive Properties Value Comments
Appearance White