Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 47.0 MPa | 6820 psi | |
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of.. |
|||
Flexural Strength | <= 47.0 MPa | <= 6820 psi | ISO 178 |
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 47.0 MPa @Temperature 23.0 °C |
6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 47.0 MPa @Temperature 23.0 °C |
6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 47.0 MPa @Temperature 23.0 °C |
6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 47.0 MPa @Temperature 23.0 °C |
6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 47.0 MPa @Temperature 23.0 °C |
6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 47.0 MPa @Temperature 23.0 °C |
6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
LG Chemical LUCEL HI-525 High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
LG Chemical LUPOL HF-3208H High Flow Polypropylene, 20% Mineral Fillers, General Purpose LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ISO 178 |
Solvay TECHNYL® A 230 PA66, Conditioned Description: Unreinforced and modified polyamide 66, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 230 offers excel.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific) LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Videolar 825 E High Impact Polystyrene (HIPS) Grade designed specially for extrusion and thermoformingCharacteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusionFeatures: St.. |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T20L1 Talc Reinforced |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L1 Talc Reinforced |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T40L1 Talc Reinforced |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336M40CL Mica Reinforced Coupled |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339T30L1 Talc Reinforced |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339T10L1 Talc Reinforced |
|||
Flexural Strength | 47.0 MPa | 6820 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339T20L1 Talc Reinforced |
|||
Flexural Strength | 47.0 MPa | 6820 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |