Material Notes:
Construction: Expanded Metal in ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Monel AluminumInformation provided by Chomerics
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Silicone Version
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
Electrical Properties Metric English Comments
Shielding Effectiveness >= 35 dB

@Frequency 14000 Hz
>= 35 dB

@Frequency 14000 Hz
>= 85 dB

@Frequency 1.00e+9 Hz
>= 85 dB

@Frequency 1.00e+9 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Descriptive Properties Value Comments
Maximum Joint Unevenness, % of Gasket Height 0.1
Class B- Open-Close in Same Position
0.1
Class C- Completely Interchangeable
0.15
Class A- Permanently Closed