Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Mytex Polymers 8224LW Polypropylene, Non-filled, Compounded Description: Mytex® 8224LW is a non-filled compounded polypropylene produced for automotive applications.Key Applications: Automotive exteriorInformation provided by Mytex Polymers |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | DIN EN ISO 197 397 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® A 238 Black 21 N PA66, Conditioned Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent .. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® B 218 Black 21 N PA66/6, Conditioned Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6 (Asia Pacific) LNP* Lubricomp* PFL36 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
Izod Impact, Notched (ISO) | >= 16.0 kJ/m² | >= 7.61 ft-lb/in² | |
Sibur ABS 0809M Molding Grade ABS Plastic Shock resistant with high thermal resistance for production of structural and decorative parts and articles of technical purpose. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF008ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180 |
Styrolution Terluran® HD-15 ABS Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180/A |
Styron EMERGEâ„¢ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON E9007E PEI LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180 |
Polyram RamSter PF300G8 PBT, 40% Glass Fiber 40% Glass fiber reinforced PBT for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FX 995 - 10% Talc/Mineral Reinforced, Impact Modified Polypropylene Copolymer Compound with High Flow 10% Mineral Reinforced, High Flow, Impact Modified PP CopolymerApplications: Automotive Pillars & TrimsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl B2 ZV20 Nylon 6, 20% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl B2 G10 V20 Nylon 6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl C2 V40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | ASTM D256 |
BLUESTAR LXS 112 PPE-PS Typical Applications: PV Industrial partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF OF006I PPS - Linear LNP THERMOTUF* OF006I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact. |