Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fatigue strength, good chemical resistance and high mechanical property retention over a broad temperature and humidity range.Features: Ductile; Good Chemical Resistance; Heat Stabilized; Hot Water Moldability; Impact Modified; Low WarpageUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal ReplacementInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PA1234 Color: BK684 Black; ASTM D4000 PA1234 Color: NT Natural; ASTM D6779 PA1234; DELPHI 23295267 Color: BK-684 Black; DELPHI 23295267 Color: NT Natural; DELPHI 28213409 Color: BK-684 Black; DELPHI 28213409 Color: NT Natural; DELPHI M-2965 Color: BK684 Black; DELPHI M-2965 Color: NT Natural; DELPHI MSP24103175 Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Dry; ISO 1183
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
Dry
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 62.7 MPa

@Temperature 23.0 °C
9090 psi

@Temperature 73.4 °F
ASTM D638
96.5 MPa

@Temperature -40.0 °C
14000 psi

@Temperature -40.0 °F
ASTM D638
Elongation at Break 11 %

@Temperature -40.0 °C
11 %

@Temperature -40.0 °F
ASTM D638
18 %

@Temperature 23.0 °C
18 %

@Temperature 73.4 °F
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Strength 85.5 MPa
12400 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
Peak; Dry; ASTM D3418
310 °C
590 °F
Dry; ISO 11357-3
Processing Properties Metric English Comments
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 110 °C

@Time 14400 sec
230 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Natural
Form Pellets
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant