Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 161J-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 161J1-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 161J-4-DD Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2188GC-1V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2188NT Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent natural PVC bottle compound for blow molding applications.Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging XPL 355GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging XPL189 Amber 1505 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Dry Blend E6755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)
(Unverified Data**) Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Izod Impact, Notched | 11.0 J/cm @Temperature 23.0 °C |
20.6 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA880 Nylon 6.6, Impact Modified Super tough - impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D265 |
Solvay TECHNYL® 1021ST PA6, DRY Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balan.. |
|||
Izod Impact, Notched | 11.0 J/cm | 20.6 ft-lb/in | ASTM D256-70 |
Budd Hi-Flex® SMC
(discontinued **) Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer. |