Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.41 GPa | 350 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/05T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC) Information provided by PolyOne |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1603-03 Polycarbonate Resin Description: LUPOY PC 1603-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1300-10 Polycarbonate Resin Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Spartech UltraTuf SG Polycarbonate Sheet Description: Polycarbonate SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and .. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D-882 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2929 Fluoropolymer Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Ecomass® 3620BX18 5% Borated Polyethylene (HDPE) 5% Borated Polyethylene (HDPE), Product Form - Pellets, No Pre-Drying RequiredProcessing Method: Injection Molding, Compression MoldingNeutron Shielding ApplicationsInformation provided by Technica.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D-638 |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Solvay Specialty Polymers Mindel® S-1000 Modified Polysulfone
(discontinued **) This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated
  Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM Data |
Styron Magnum™ 9100 MFD ABS Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | TM R050-36 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Conditioned; ASTM D638 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |