Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.5 MPa | 12400 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0111 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 85.8 MPa | 12400 psi | ASTM D790 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Strength | 85.5 MPa @Thickness 3.18 mm, Temperature 23.0 °C |
12400 psi @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D790 |
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 85.5 MPa | 12400 psi | ASTM D790 |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Flexural Strength | 85.5 MPa | 12400 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Flexural Strength | 85.3 MPa | 12400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 85.3 MPa | 12400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 85.8 MPa | 12400 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY PCPBT 2525 PC/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 85.5 MPa | 12400 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M4910 (USP CLASS VI for TRANS 9494 only) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 85.5 MPa | 12400 psi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)