Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.41 GPa | 350 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC) Information provided by PolyOne |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® X37 ABS ABS, injection moulding, high heat grade.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® EHA PC+ABS (Asia Pacific) PC+ABS. Electroplateable. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP 300 TFE 15 Polycarbonate (PC), PTFE Lubricated |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® SY-03CF/000 Polystyrene - High Impact (HIPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1603-03 Polycarbonate Resin Description: LUPOY PC 1603-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1303-07 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS (Asia Pacific) LNP* Stat-kon* AX06518 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, Fl.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Star Plastics PC703 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Star Plastics PC741 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl N750T PPE+HIPS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company EMI 661 FR A Acrylonitrile Butadiene Styrene (ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP 2500 A TFE 10 Polycarbonate/ABS Alloy (PC/ABS), PTFE Lubricated |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP 2500 TFE 5 Polycarbonate/ABS Alloy (PC/ABS), PTFE Lubricated |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP 300 AR 10 TFE 10 Polycarbonate (PC), Aramid Fiber - PTFE Lubricated |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP 300 LF FR A UV Polycarbonate (PC), Low Flow - Unreinforced - Flame Retardant - UV Stabilized - UL94 V-0 The RTP 300 FR A family of materials offer dimensional stability, rigidity, heat resistance, ignition resistance and excellent impact strength. RTP 300 LF FR A UV is a UV-stabilized grade designed .. |
|||
Tensile Modulus | 2.41 - 2.76 GPa @Temperature 23.9 °C |
350 - 400 ksi @Temperature 75.0 °F |
|
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
CRG Industries Essemplex AB43 Thermoplastic Shape Memory Polymer Resin Essemplex is a melt-processible shape memory polymer (SMP) resin. Its unique properties offer versatile design options for reconfigurable and customizable products. Essemplex is compatible with curr.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6) Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D-638 |
Axiall 6680 Rigid PVC, Molding, White 476 Georgia Gulf 6680 White 476 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, s.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D-638 |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-20GB/15T Acetal-Copolymer, Glass Bead Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D-638 |
Axiall 9202J Rigid PVC, Molding Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive produ.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP 399 X 120436 C Polycarbonate (PC), Carbon Nanotube |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP 399 X 86846 H Polycarbonate (PC) Flame Retardant - Halogen Free - Transparent |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | TM R050-36 |
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D 638 |
RTP Company RTP PA6 HI NAT Nylon 6 (PA), Impact Modified - Value Product |