Category Polymer , Thermoplastic , Nylon
Manufacturer Samyang
Trade Name Tramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Tramid® 210G35 Polyamide, Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G35 is a reinforced grade.Applications:Automotive gear level housingConnectorsIntake manifoldsThermostat housingCooling radiator modulesSprinklerWater pipesFan and shroudECU casesCylinder head coverIndustrial ball valveInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 196 MPa
28400 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 260 MPa
37700 psi
ASTM D790
Flexural Modulus 8.97 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 1.18 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 21.0 kV/mm
533 kV/in
ASTM D149
Users viewing this material also viewed the following: