Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.41 - 1.43 g/cc | 1.41 - 1.43 g/cc | ISO.1183 DN.53479 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Ovation Polymers Nemcon™ E PET 30131 PET PET-Fiber Grade with ESD Range Conductivity with improved processability. Information provided by Ovation Polymers |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | "B" component |
ACC QSil 430 QSI Quantum Silicones Silicone Potting Material
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, quick curing, flame retardant, great adhesion to a variety of substrates. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin Improved weather resistance and low odor of FA. Applications: Weather resistant products at closed space. Information provided by API-Kolon. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Loxim 200 00V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ISO 1183 |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | |
Momentive Performance Materials FSE7570-D1 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | |
Sylvin Technologies 9960-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12 LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI) TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | |
Aremco Ceramabind™ 642 High Temperature Inorganic Binder A basic solution which is highly compatible with most ceramic and metal powders. Good wettability and tack, and excellent acid resistance after curing. Extremely moisture resistant after a high temp.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7825 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |