Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylex® P1010G7FRMA Polycarbonate, 7% Glass Filled Polycarbonate, 7% Glass Filled, Flame RetardantInformation provided by Ravago. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Total 819E Polystyrene
(discontinued **) Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Global B-6200 High Density Polyethylene Description-suitable for high quality blow molding, provides excellent surface glossiness in combination w/ outstanding environmental stress cracking resistanceApplications-cosmetics bottles, shampo.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE GF30 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good UV ResistanceAdditive: UV StabilizerInformation provided by TP Composites.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF30 HS UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF33 L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackTPCI# 8221102Information provid.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF33 L N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: Fast Molding Cycle and LubricatedAppearance: BlackTPCI# 87.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessin.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 HS L BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
SK Chemicals SKYPEL G172D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® VGR10 10% GF ABS Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Washington Penn Medium Impact Copolymer 50% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S519 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® J910 10% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature 22.8 °C |
2.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Aclo Accutech ABS ABS834G10L Glass Reinforced |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437T20L Talc Reinforced |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |