Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66 G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Global B-6200 High Density Polyethylene Description-suitable for high quality blow molding, provides excellent surface glossiness in combination w/ outstanding environmental stress cracking resistanceApplications-cosmetics bottles, shampo.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® SM850 Polypropylene impact copolymer Titanpro® SM850 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® SM950 Polypropylene impact copolymer Titanpro® SM950 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
Kolon Kopa® KN163G30 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | >= 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.20 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL LW4302 PP+GF/MF30% Description: Injection Molding, PP+GF/MF30%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 14807-96-6 and 165997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411H PC LNP* THERMOCOMP* DX06411H is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9120AT ASA, Unreinforced Used in washing machine cover etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tramid® 210G35 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G35 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | |
Zylog Hipolyene® 6251 Y Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | |
Zylog Hipolyene® 9221 XM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T885GV3 Flame Retardant PBT, 30% Glass Fiber |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® J910 10% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | Wet; ASTM D256 |
Asahi Kasei Leona® FR200 Nylon 66 UL94 V-0; halogen-free and phosphor-free.Applications:Connectors, switches, and other electrical and electronic parts Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Asia Technology Pioneers CAP 702 PP Nanocomposite Description: CAP702 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G7F Nylon 66, 35% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® C130GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
Kolon Kopa® KN153G15 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |