Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 196 MPa | 28400 psi | ASTM D638 |
Quantum Composites HTC-9500 55% E-Glass Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9500 (127-51-6) is an E-Glass Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics providing .. |
|||
Tensile Strength | 196 MPa | 28400 psi | ASTM D638 |
Samyang Tramid® 210G35 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G35 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Tensile Strength | 196 MPa | 28400 psi | 50 mm/min; ISO 527 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |