SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Density 1.328 g/cc
0.04798 lb/in³
ASTM D792
Moisture Absorption 0.500 %
0.500 %
50% RH, 24 hrs; ASTM D570
Moisture Absorption at Equilibrium 1.0 %
1.0 %
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0065 - 0.0085 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0085 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 158 MPa
22900 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 151 MPa
21900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 7.0 %
7.0 %
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 248 MPa
36000 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 8.58 GPa
1240 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 1.06 J/cm
1.99 ft-lb/in
ASTM D256
0.800 J/cm

@Temperature -30.0 °C
1.50 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 - 30.6 µm/m-°C

@Temperature -20.0 - 150 °C
11.0 - 17.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 254 °C

@Thickness 6.40 mm
489 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 240 °C

@Thickness 6.40 mm
464 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 248 °C
478 °F
Rate B/50; ASTM D1525
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
122 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI 30 - 60 arcs
30 - 60 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A