Polymer Property : Density = 1.328 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.328 g/cc
0.04798 lb/in³
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA
30% Glass Reinforced PPE+PA Alloy.
Density 1.328 g/cc
0.04798 lb/in³
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific)
GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet.
Density 1.328 g/cc
0.04798 lb/in³
JIS-Z-8807
Denka VINYKON W5520 PVC, W grade for non-migratory sheath and special items
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..