Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3413R PC (Asia Pacific) Lexan* resin 3413R is a flame retardant polycarbonate grade with 30% glass fiber reinforcement to meet UL 94 V1 listing at 1.5mm. This grade can be considered for applications requiring higher stiff.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3433R PC 30% GR, provides improved mechanical properties. UV-stabilized. Internal mold release. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 500 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXM121R PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Izod Impact, Notched | 1.06 - 6.94 J/cm | 1.99 - 13.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | Method A; ASTM D256 |
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high stren.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Izod Impact, Notched | 1.06 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
1.99 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Ravago Manufacturing Americas Echo® RPPC 30/2 BK Recycled Polypropylene Copolymer Polypropylene, Unreinforced, 30 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, .. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific) PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66 LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubriloy Z2000 PPE+PS LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP fo.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AX05466H ABS (Asia Pacific) LNP* THERMOCOMP* AX05466H is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp PH0700B PA 6 LNP* Thermocomp* PH0700B is a Nylon 6 base resin containing Tungsten. Characteristics are High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXQ PA 66 LNP THERMOCOMP* RF007SXQ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Hydrolysis Resistant. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA 30% Glass Reinforced PPE+PA Alloy. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific) 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile .. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412HF PC (Asia Pacific) 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6 LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |