Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3413R PC 30% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXM121R PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | Method A; ASTM D256 |
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high stren.. |
|||
Izod Impact, Notched | 1.06 - 2.12 J/cm | 1.99 - 3.97 ft-lb/in | |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC (Asia Pacific) LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -40.0 °C |
1.99 ft-lb/in @Temperature -40.0 °F |
|
Metton LMR M1534 Liquid Molding Resin Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce .. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific) PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific) LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPE+PS (Asia Pacific) LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC (Asia Pacific) LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON PFD06 PA 6 (Asia Pacific) LNP* Stat-kon* PFD06 is a compound based on Nylon 6 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific) LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXQ PA 66 LNP THERMOCOMP* RF007SXQ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Hydrolysis Resistant. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific) GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific) 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp DF0066P PC LNP THERMOCOMP* DF0066P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing.This data was supplied by.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers VESPEL TP-8549 Polyimide Thermoplastic parts from filled PI (polyimide) for high mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance.. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile .. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |