Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 3413R PC (Asia Pacific) Lexan* resin 3413R is a flame retardant polycarbonate grade with 30% glass fiber reinforcement to meet UL 94 V1 listing at 1.5mm. This grade can be considered for applications requiring higher stiff.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 6.60 mm |
>= 120 sec @Thickness 0.260 in |
UL 746 |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | PLC code 0; UL 746A |
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | PLC code 0; UL 746A |
SABIC Innovative Plastics Valox® CS860 PBT+PET (Asia Pacific) 30% glass reinforced PBT+PET blend. Color stable, FR. Housewares, appliances; iron skirt, oven trim/panels.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4111 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain Reliefs; Wire and Cable ApplicationsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Comp.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 6500-105 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Extrusion Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Compon.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.05 mm |
>= 120 sec @Thickness 0.120 in |
UL PLC 0 (120+ sec) |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+PS LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |