SABIC Innovative Plastics LNP COLORCOMP R1000 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP R1000 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* COLORCOMP* R1000 is an unfilled Nylon 66.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.012 cm/cm
0.012 in/in
SABIC Method
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 79.0 MPa
11500 psi
5 mm/min; ISO 527
Elongation at Break 45 %
45 %
5 mm/min; ISO 527
Elongation at Yield 11 %
11 %
5 mm/min; ISO 527
Tensile Modulus 2.99 GPa
434 ksi
1 mm/min; ISO 527
Flexural Strength 33.0 MPa
4790 psi
ISO 178
Flexural Modulus 2.90 GPa
421 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 140 kJ/m²
66.6 ft-lb/in²
80*10*4; ISO 180/1A
Charpy Impact, Notched 16.5 J/cm²
78.5 ft-lb/in²
ISO 179/2C
13.9 J/cm²

@Temperature -30.0 °C
66.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/2C
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af