Covestro Texin® 4215 Urethane Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Covestro
Trade Name Texin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Texin® 4215 Urethane Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa

@Strain 50.0 %
3050 psi

@Strain 50.0 %
Elongation at Break >= 50 %
>= 50 %
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 115 µm/m-°C

@Temperature 20.0 °C
63.9 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
Vicat Softening Point 140 °C
284 °F
50°C/h 50N
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL Recognized
Processing Properties Metric English Comments
Melt Temperature 230 °C
446 °F
Injection Molding
Mold Temperature 35.0 °C
95.0 °F
Injection Molding
Injection Pressure 45.0 MPa
6530 psi