Clariant Renol N6 15% Moly MOS2 Concentrate of Molybdenum Disulfide

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol N6 15% Moly MOS2 Concentrate of Molybdenum Disulfide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application to Nylon 6, Nylon 66Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Relative Viscosity 50 cP
50 cP