Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 140 kJ/m² | 66.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP COLORCOMP R1000 PA 66 LNP* COLORCOMP* R1000 is an unfilled Nylon 66. |
|||
Izod Impact, Notched (ISO) | >= 140 kJ/m² | >= 66.6 ft-lb/in² | Requirement |
Westlake Plastics Lennite® GUR1020 (Type I) Ultra-high Molecular Weight Polyethylene For Medical Applications Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m.. |