Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.99 GPa | 434 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | ASTM D638 |
SABIC PS 155 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 155 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and go.. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | ASTM D638 |
SABIC PS 160 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular .. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Tensile Modulus | 2.99 GPa @Temperature 23.0 °C |
434 ksi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC MC500 Polyvinyl Chloride, Chlorinated (CPVC) The Geon MC500 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon MC500 demonstrates superior processa.. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX Ultra LA427Plus Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties based on Geon HTX Ultra LA427Plus Natural 0000Information provided by PolyOne |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP R1000 PA 66 LNP* COLORCOMP* R1000 is an unfilled Nylon 66. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s). |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP LNP* THERMOCOMP* MFB71L is a compound based on Polypropylene resin containing 35% Glass Bead, 5% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP (Asia Pacific) LNP* Thermocomp* MFB71L is a compound based on Polypropylene resin. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 2.99 GPa | 434 ksi | ASTM D-638 |
Axiall 9190 Rigid PVC, Molding Georgia Gulf 9190 was developed to aid compliance with source reduction initiatives especially when low temperature impact strength is a concern. It has superior properties, which in most cases wil.. |