Premix Thermoplastics PRE-ELEC® 12-031  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRE-ELEC® 12-031  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRE-ELEC 12-031 is a conductive thermoplastic compound based on a polyacetal copolymer with 10% carbon fiber. PRE-ELEC 12-031 exhibits excellent mechanical properties and electrical conductivity. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.0 MPa
9570 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527
Izod Impact, Notched 0.580 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
1.09 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched 3.70 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
6.93 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75/Method Bf
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
ISO 75/Method Af
Electrical Properties Metric English Comments
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ISO D-257
Surface Resistance <= 1e+05
<= 1e+05
ISO D-257
Static Decay <= 2.0 sec
<= 2.0 sec
ISO IEC 61340-5-1
Processing Properties Metric English Comments
Melt Temperature 185 - 210 °C
365 - 410 °F
Mold Temperature 80.0 - 105 °C
176 - 221 °F
Drying Temperature 80.0 °C

@Time 10800 - 14400 sec
176 °F

@Time 3.00 - 4.00 hour
Pre-drying in a dehumidifier
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Descriptive Properties Value Comments
Injection Speed Moderate
Users viewing this material also viewed the following: