Processing Properties Metric English Comments
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Premix Thermoplastics PRE-ELEC® PP 1373
PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® M90SW POM, Tribological  (Unverified Data**)
Celcon M90SW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear against the same mating surface is important. This grade may be preferre..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® MC90-HM POM, Mineral Reinforced  (Unverified Data**)
Celcon® MC90-HM is a highly mineral filled and coupled M90 material for producing very flat and dimensionally stable parts (normal flow).Mineral coupled for reduced warpage, high modulus, moderate ..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 13031 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with moderate flow, about 10% higher strength, rigidity and hardness than C 13021Information provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 2521 G POM, Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMStiff-flowing grade for injection molding and extrusion, modified with (R) GUR (PE-UHMW)Information provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 26 % glass fibersInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® MR130HPB POM, Specialty  (Unverified Data**)
Preliminary Data SheetMedia resistant - bleach, high modulus gradeInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® WR140LG POM, UV Resistant  (Unverified Data**)
Hostaform® acetal copolymer grade WR140LG Black is a specialty weatherable grade of acetal copolymer formulated to provide good flow with a low gloss finish and a UV stability necessary for exterio..
Injection Pressure 60.0 MPa
8700 psi
Ineos ABS Centrex® 821 ASA Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection ..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Average value: 86.5 MPa Grade Count:4
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
Injection Pressure 60.0 MPa
8700 psi
Covestro Makroblend® UT-403 Polycarbonate + Polyester Blend
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celstran® PP-GF50-0403 P10 PP, 50% Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 52021 POM, Unfilled
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® LM90 POM, Specialty
Hostaform« LM90 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform« LM90 can be laser marked with barcodes, identif..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® MT12U03 POM, Medical Technology
Hostaform« MT12U03 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform« MT12U03 is a moderately high flow grade for fa..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified
POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® S 9362 XAP2 ™ POM, Impact Modified
Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® M450 POM, Unfilled
Celcon« acetal copolymer grade M450 is an extremely low viscosity grade for optimal cycle performance in very thin walls or long, narrow flow paths in injection molding.Information provided by Cela..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celstran® PP-GF30-0405 P10/10 PP, 30% Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celstran® PP-GF40-0455 P10/10 PP, 40% Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celstran® PP-GF50-0453P10/10 PP, 50% Glass Reinforced
Material code according to ISO 1043-1: PPlow emission materialCelstran can be processed on a standard injection molding unit.Information provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® S 9364 WS 10/1570 POM, UV Resistant
Preliminary Data SheetInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 9021 M XAP2® POM
Description: Injection molding type, modified with molybdenum disulphide; good chemical resistance to solvents, fuel and strong alkalis as well as good hydrolysis resistance; high resistance to ther..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Beijing Ranger Chem PBT-201-G20 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Celcon® MR90B POM, Specialty  (Unverified Data**)
Celcon® MR90B is a standard flow specialty media resistant grade developed for improved bleach resistance.Improved media resistance, standard grade.Standard reciprocating screw injection molding ma..
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® XT 20 POM, Impact Modified  (Unverified Data**)
Preliminary Data SheetHighly Impact ModifiedInformation provided by Celanese
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Celanese Hostaform® C 27021 XAP² ™ LS colored POM, UV Resistant
PolyacetalcopolymerInformation provided by Celanese